REFINEIT-10MK Electrolytic Gold and Silver Refining System. 0.5 Kilo (15 oz) per Day

$4,490.00

Product Number: RFx10MSx

REFINEIT-10MK is a multifunctional, small-footprint electrolytic system, designed to refine gold and silver. Where the gold refining process has historically been lengthy and involved, our innovative process reduces gold refinement to a single step. Refining gold in REFINEIT requires four times less acids, this acid being diluted, and requires no chemicals beside nitric acid. REFINEIT-10M refines gold by dissolving and removing all base metals from the gold alloy (electroparting), without dissolving the gold itself

Once the process is complete, your 24K gold is ready for use inside of anode compartment. No additional manipulations.

REFINEIT-10M will refine any type of gold except computer boards. Gold-filled items must be mixed with solid karat gold before refining. REFINEIT will provide the best gold return with the lowest consumption of chemicals, and will reduce the entire process to a single, simple step, minimizing the need for human involvement. REFINEIT is consuming four times less acids then common Aqua Regia procedure.

Our latest proprietary protocol will refine gold with very little toxic fumes produced. It will be even possible to refine gold alloys with absolutely no toxic fumes produced! Instead our system will produce oxygen!

* REFINEIT-10M requires adequate ventilation and proper chemicals handling. Although Fumeless technology will provide high level of protection against toxic fumes, still REFINEIT equipment should be operated in vented area for additional protection.

Brief Description of Gold Electroparting Protocols:

For 2K to 10K gold:

  • Melt your 2K - 10K gold and cast an ingot
  • Place gold ingot into the unit, fill the unit with electrolyte and turn on power supply
  • 12-24 hours later, remove anode section and wash refined gold with water
  • Remove refined gold from anode section
  • Use refined gold

For 10K and more gold:

  • Melt your gold with copper, or with gold-filled items to make it 6K to 8K, and cast an ingot
  • Place gold ingot into the unit, fill the unit with electrolyte and turn on power supply
  • 12-24 hours later, remove anode section, wash the gold with water
  • Remove refined gold from anode section
  • Use refined gold

Specifications

Model REFINEIT-10M
Capacity 5-15 oz gold alloy per cycle
Operation Time Up to 24 hour per cycle, depends on the load
Power Rating DC, Max 4 volt, 10 ampere, 40 Watt
Gold Purity 99.5 % +
Chemicals Nitric acid
Consumables Nitric acid
Dimensions 12" L x 6" W x 8" H
Weight 17 lb, 30 lb with power supply
Included Main unit
2 cathode sections with replaceable membranes
Anode section with replaceable membranes
2 cathode plates
Anode and cathode connection wires.
Anode connection clip
Safety tray with integrated drain valve
Instruction

Reviews

There are no reviews yet.

Only logged in customers who have purchased this product may leave a review.